Abstract:
Waste tyres pyrolysis (WT- pyrolysis) process provides a sustainable  solution for waste tyre recycling. Value addition to pyrolytic tyre char (PT char) is particularly essential because it will reduce enormous inventories of  wasted PT-char, generate income, and enhance WT-pyrolysis sustainability  while still being environmentally friendly. This study was aimed at  modifying the surface properties of unusable PT-char to be amalgamated in a  rubber compound. PT-char was obtained from a WT-pyrolysis plant, sieved,  demineralized using diluted HCl and or Citric acid followed by diluted  NaOH. The purified samples were then heated with different ratios of 92- 
octane at 220-250 °C until the self-ignition of octane occurred. The heat  produced by the self-ignition triggered the activation of the surface of PT char as well as it initiated localized explosions which resulted in breaking up  the large PT-char particles.